Niblend S45 HG

Produkt anfragen   Datenblatt herunterladen    Telefonische Beratung +49 40 727702-0

PC-ABS alloy of medium-high thermic resistence for the injection moulding of items

Requiring good aesthetic characteristics.

PropertiesTest conditionMethodUnitValue
RheologicalMelt Flow Index260°C / 5 kgASTM D1238g/10min20
MechanicalTensile Stress at Yield50 mm/min.ASTM D638MPa40
MechanicalFlexural Maximum Stress1,3 mm/minASTM D790MPa65
MechanicalFlexural Elastic Modulus1,3 mm/minASTM D790MPa2300
MechanicalRockwell HardnessASTM D785R-scale115
MechanicalIzod Notched Impact Strength23°C/3,2 mmASTM D256J/m400
MechanicalIzod Notched Impact Strength-20°C/3,2 mmASTM D256J/m120
MechanicalElongation50 mm/minASTM D638%30
ThermalVicat Softening Temperature49N / 120°C/hASTM D 1525°C117
ThermalHeat Distortion Temperature H.D.T1.82 MPaASTM D648°C106
ThermalCoef. Dilatazione Termica Lineare23/55 °CISO 11359-210^-5 K^-18
Flame BehaviourGlow Wire Temperature (G.W.T)S=2.0 mmIEC 695-2-1°C650
Flame BehaviourUL 94 RatingS=1.6 mmUL 94classHB
Flame BehaviourUL 94 RatingS=3.2 mmUL 94classHB
ElectricalDielectric StrengthS=1 mmIEC 60243-1KV/mm25
ElectricalRelative Permettivity1 Mhz = seccoIEC 60250-2,9
ElectricalDissipation Factor1 Mhz = seccoIEC 60250-0,05
ElectricalSurface ResistivityseccoIEC 60093Ω10^15
ElectricalVolume ResistivityseccoIEC 60093Ω • cm10^15
VariousDensityASTM D792g/cm³1,1
VariousHumidity Content at Equilibrium23°C / 50 % U.R.ISO 62%0,2
VariousMoulding Shrinkageparallel-%0,5-0,8