Niblend S65 HG

Produkt anfragen   Datenblatt herunterladen    Telefonische Beratung +49 40 727702-0

PC-ABS alloy of hich-thermic resistance for the injection moulding ok glossy items.

PropertiesTest conditionMethodUnitValue
RheologicalMelt Flow Index260°C / 5 kgASTM D1238g/10min20
MechanicalTensile Stress at Yield50 mm/min.ASTM D638MPa45
MechanicalFlexural Maximum Stress1,3 mm/minASTM D790MPa70
MechanicalFlexural Elastic Modulus1,3 mm/minASTM D790MPa2300
MechanicalIzod Notched Impact Strength23°C/3mmASTM D256J/m450
MechanicalIzod Notched Impact Strength-20°C/3mmASTM D256J/m150
MechanicalRockwell Hardness23°CASTM D785M-scale115
MechanicalElongation50 mm/minASTM D638%30
ThermalVicat Softening Temperature49N / 120°C/hASTM D 1525°C125
ThermalHeat Distortion Temperature H.D.T1.82 MPaASTM D648°C112
ThermalLinear Expansion Coefficient23°C/55°CISO 11359-210^-5 K^-18
Flame BehaviourGlow Wire Temperature (G.W.T)S=2.0 mmIEC 695-2-1°C650
Flame BehaviourUL 94 RatingS=1.6 mmUL 94classHB
Flame BehaviourUL 94 RatingS=3.2 mmUL 94classHB
ElectricalRelative Permettivity1 Mhz – dryIEC 60250-2,9
ElectricalDissipation Factor1 Mhz – dryIEC 60250-0,05
ElectricalDielectric StrengthS=1 mmIEC 60243-1KV/mm25
ElectricalSurface ResistivitydryIEC 60093Ω10^15
ElectricalVolume ResistivitydryIEC 60093Ω • cm10^15
VariousDensityASTM D792g/cm³1,12
VariousHumidity Content at Equilibrium23°C / 50 % U.R.ISO 62%0,2
VariousMoulding Shrinkageparallel-%0,5 – 0,8